VALUE METAL INDUSTRY CO.,LTD. specializes in all kinds of soft materials with normal hardness and high hardness or ultra-high hardness stainless steel (SUS304, 301, 430), tinplate, nickel alloys and special metals such as copper and copper alloys.
materials; and specializes in importing foreign metal materials from Japan, South Korea and other countries to serve customers all over the world. Available in thicknesses from 0.005 mm ~ 3mm, with complete operating modes and consistent production processes, please call us for enquiries.
Schematic diagram of main stainless steel products
Chemical composition of stainless steel
Type
Steel Grade
C%
Mn%
P%
S%
Si%
Cr%
Ni%
Mo%
鐵系
鋼種
碳C
錳Mn
磷P
硫S
矽Si
鉻Cr
鎳Ni
鉬Mo
main purpose
奧斯田鐵系 AUSTENITIC
SUS 301
≦0.15
≦2
≦0.045
≦0.03
≦1.00
16.00-18.00
6.00-8.00
Good ductility for molded products
SUS 304
≦0.08
≦2
≦0.045
≦0.03
≦1.00
18.00-20.00
8.00-12.00
Has good heat resistance The most widely used
SUS 304L
≦0.03
≦2
≦0.045
≦0.03
≦1.00
18.00-20.00
8.00-12.00
Products that are less susceptible to heat treatment
SUS 305
≦0.12
≦2
≦0.045
≦0.30
≦1.00
17.00-19.00
10.00-13.00
Use more non-magnetic products
SUS 316
≦0.08
≦2
≦0.045
≦0.03
≦1.00
16.00-18.00
10.00-14.00
2.00-3.00
SUS 316L
≦0.03
≦2
≦0.045
≦0.03
≦1.00
16.00-18.00
10.00-14.00
2.00-3.00
Corrosion resistance Easy to heat treat
肥粒鐵系 FERRITIC
SUS 430
≦0.12
≦1
≦0.040
≦0.03
≦1.00
14.00-18.00
Good formability But poor heat resistance and corrosion resistance
Stainless steel mechanical properties
Material
Hardness
Hardness range
Yield Strength(YS) N/mm2
Tensile Strength(TS) N/mm2
延申率% Elongation
301
1/2 H
310 min
510 min
930 min
10 min
3/4 H
370 min
745 min
1130 min
5 min
H
430 min
1030 min
1320 min
3 min
EH
490 min
1275 min
1570 min
-
SEH
530 min
1450 min
1740 min
-
304
1/2 H
250 min
470 min
780 min
6 min
3/4 H
310 min
665 min
930 min
3 min
H
370 min
880 min
1130 min
-
302
SOFT
200 max
205 min
520 min
40 min
305
SOFT
200 max
175 min
480 min
40 min
316L
SOFT
200 max
175 min
480 min
40 min
409
SOFT
175 max
175 min
360 min
22 min
410
SOFT
210 max
205 min
440 min
20 min
420J2
SOFT
247 max
225 min
540 min
18 min
429
SOFT
200 max
205 min
390 min
25 min
430
SOFT
200 max
205 min
450 min
22 min
436
SOFT
200 max
-
410 min
22 min
It is made by tin-plating the surface of steel plates. It has the advantages of anti-rust and corrosion resistance. It is suitable for welding and is a widely used material. It is mainly used for canning (and suitable for painting, coating, printing) and electronic industry parts. and other material applications.
Amount of tin plating on tinplate surface
Symbol
Type
Symbol
Nominal Surface tin amount
minimum average Surface tin amount
SPTE
Equal Coating
CNS
JIS
g/m²
lb/B.B.
g/m²
lb/B.B.
1.1/1.1
#10
1.1/1.1
0.05/0.05
0.9/0.9
0.04/0.04
2.8/2.8
#25
2.8/2.5
0.125/0.125
2.45/2.45
0.11/0.11
5.6/5.6
#50
5.6/5.6
0.25/0.25
5.05/5.05
0.23/0.23
8.4/8.4
#75
8.4/8.4
0.375/0.375
7.55/7.55
0.35/0.35
11.2/11.2
#100
11.2/11.2
0.50/0.50
10.1/10.1
0.45/0.45
Differential Coating
2.8/5.6
#25/50
2.8/5.6
0.125/0.25
2.45/5.05
0.11/0.23
2.8/8.4
#25/75
2.8/8.4
0.125/0.375
2.45/7.55
0.11/0.35
2.8/11.2
#25/100
2.8/11.2
0.125/0.50
2.45/10.1
0.11/0.45
5.6/8.4
#50/75
5.6/8.4
0.25/0.375
5.05/7.55
0.23/0.35
*Indicates that the tin content on both sides is different. D-mark and A-mark can be used to distinguish the tin content on the two sides according to customer needs
*Tin plate negative and tin plated steel symbol
Type
Symbol
Material negative
SPB
Electroplated tin plated steel sheet
SPTE
Hot dipped tin plated steel sheet
SPTH
Product name
Specifications and dimensions (currently of our company)
Tinplate
0.15mm~0.6mm
Temper Designation
Symbol
Rockwell hardness target value (HR-30)
Usage
Single Reduced
T1
46~52
Drawn requirements,nozzles,spouts,closures
T2
50~56
Applications where moderate drawability and some stiffness are required small square and oval
T2.5
52~58
Items requiring the drawability of T2 in combination with the stiffness of T3
T3 T3CA
54~60
Can ends and bodies,large diameter closures,crown caps
T4CA
58~64
General line cans,crowns and others requiring higher stiffness than T3
T5CA
62~68
Large can ends and bodies where excellent bulking resistance is required
Double Reduced
DR-8CA
70~76
Can body for beers and carbonated beverages
DR-9CA
73~79
Large can body,can ends
*T1 Soft materials with emphasized workability can be used for deep drawing
*T2 High performance for deep drawing
*T2.5 It is a balanced and elongation type located between T-2 and T-3
*T3 For general use and elongation
*T4CA Continuously annealed single-pass cold-rolled products have higher toughness and are suitable for cans, barrels, and tops
*T5CA T5CA Continuously annealed single-pass cold-rolled products, considered when buckling resistance is required
*CA is continuously annealed and has the advantages of high hardness, uniform mechanical properties and high corrosion resistance
*R-8CA、DR-9CA The original plate is annealed and then rolled again into extremely thin and strong tinplate
Tinplate secondary rolled products
Double Reduced
hardness HR30T Rockwell hardness
Carrying capacity Rolling Direction N/mm2
DR-8
73±5
550
DR-9
76±5
620
DR-9M
77±5
660
DR-10
80±5
690
*DR-1 Annealed, it can be used as body panels for round cans that require rigidity and strength
*DR-8 Also suitable for applications requiring greater strength, such as round tank roofs and floors
*DR-9 Has the strongest annealability of tinplate and is used for special applications
Tinplate surface treatment
Mark
Classification
Specific Features
Single Reduction
B
Smooth Finish
On a substrate with a fine-grained smooth surface, the tin layer is applied to a melt-processed glossy surface
R
Stone Finish
On the negative film with a certain direction of the whetstone surface, the tin layer is applied to a melt-processed glossy surface
S
Silver Finish
On a substrate with a coarse matte surface, the tin layer is applied to a melt-processed glossy surface
M
Matt Finish
A matte surface usually obtained by tinting a matte-surface substrate without melting it
Double Reduction
R
Super Stone Finish
Tin plating is applied to the base plate with certain millstone particles and melted to give it a glossy finish
Nickel-Silver
Alloy composition(%)
Characteristics and uses
Cu
Mn
Fe
Zn
Ni
Pb
C7701
54.0-58.0
≤0.50
≤0.25
remnant
16.5-19.5
≤0.03
Beautiful color High tensile strength Good elongation for deep drawing Anti-fatigue, excellent elasticity Anti-corrosion properties
C7521
62.0-66.0
≤0.50
≤0.25
remnant
16.5-19.5
≤0.03
Material has excellent toughness And it has a bright silvery white color and stability Suitable for mobile phone shielding cover Electronic communication and other shielding collar
Tensile Strength
Elongation
Yield Strength(MPa)
Hardness
Conductivity
Thermal conductivity
Elastic coefficient
(N/mm2)
(%)
(HV)
(%IACS)
(Cal/cm2/cm/sec/°C)
(KN/mm2)
C7701
1/2H
540-655
150-210
540
140-200
≥ 5.5
H
630-735
180-240
635
175-220
EH
705-805
210-260
715
195-240
SH
760-860
230-270
785
210-250
C7521
1/2H
440-570
120-180
540
130-160
≥ 6
H
540-640
150-210
635
150-180
 
HEAD OFFICE / SHULIN PLANT
886-2-8970-2849
886-2-8970-2861
value.metal@msa.hinet.net
No.5,Ln436,Bade St.,Shulin Dist.,
New Taipei City 23857,Taiwan(R.O.C)
SOUTHERN OFFICE / TAINAN PLANT
886-6-255-5577
886-6-255-0707
No.35,Anxin 6th Rd.,Annan Dist.,Tainan City 709007,Taiwan(R.O.C)